GPCIn Stock

GPC

GPCCarbon Products

Graphitized Petroleum Coke (GPC) is a recarburizer produced by heat-treating petroleum coke at graphitization temperatures, which orders the carbon into a graphitic lattice. That structure gives fast, high-efficiency dissolution in molten iron and steel and minimal nitrogen pickup, useful where low-N carbon control matters. With F.C ≥ 98.5% and S ≤ 0.05%, GPC raises carbon without loading sulphur, supporting clean nodule formation in ductile iron and consistent matrix carbon in grey iron. It serves ductile and grey iron casting, steel carburization, and brake pad/friction material formulations. Typical recarburizer additions run roughly 0.3-2.0 wt% of charge, set by base carbon and target chemistry, with high recovery from the graphitic structure. The 1-5 mm sizing and ≤ 0.5% ash, V.M, and moisture suit ladle and in-furnace additions with stable yield. Each lot ships with COA and MTC; F.C, S, and ash are verified per shipment. Multi-regional sourcing supports CIF Marmara delivery in 20 MT FCL. Send your target grade and tonnage for an RFQ.

Technical Specifications

F.C≥ 98.5%S≤ 0.05%Ash≤ 0.5%V.M≤ 0.5%

Applications

Ductile ironGrey ironSteel carburization
Details
Recarburizer (Calcined Petroleum Coke)Out of StockNEW

Recarburizer (Calcined Petroleum Coke)

CPCCarbon Products

Calcined Petroleum Coke (CPC) is a carbon raiser used to set and correct carbon content in molten iron and steel. Calcination drives off volatiles and orders the carbon structure, yielding a dense material with ≥ 98.5% fixed carbon, ≤ 0.5% S, ≤ 0.5% ash and ≤ 0.7% V.M. Dissolved in the melt, that carbon raises the C level and feeds graphite nucleation, which governs strength and machinability in cast iron. Foundries pouring grey and ductile iron use it for carbon adjustment heat after heat, and EAF mills recarburize the charge and run it as part of slag-foaming carbon practice. Typical additions run roughly 0.5-2.0 wt% in cast iron, with charge-level dosing in steelmaking, tuned to bath temperature and target C. The 1-5 mm sizing supports steady dissolution and high recovery with low fume. Low sulphur protects nodularity in ductile grades and limits desulphurization load. Each lot ships with COA. Multi-regional sourcing supports CIF Marmara delivery, 20 MT FCL. Send your grade and tonnage for an RFQ.

Technical Specifications

F.C≥ 98.5%S≤ 0.5%Ash≤ 0.5%V.M≤ 0.7%

Applications

Cast iron carburizationGrey & ductile ironEAF steelmaking
DetailsAvailable on Request
Graphite Electrodes (UHP)Out of StockNEW

Graphite Electrodes (UHP)

Graphite ElectrodeCarbon Products

Ultra-high-power (UHP) graphite electrodes are needle-coke-based conductors that carry the high secondary current into electric arc and ladle furnaces, sustaining the arc that melts steel scrap. The graphitized needle-coke matrix gives low electrical resistivity (≤ 5.8 µΩ·m) and high bulk density (≥ 1.68 g/cm³), so the column runs cooler at high amperage, oxidizes more slowly, and resists thermal shock during charge cycling. Lower resistivity means less I²R loss and lower specific electrode consumption per tonne of liquid steel. Primary use is EAF steelmaking and ladle furnace (LF) refining, plus submerged-arc furnaces and foundry melting. Diameters span 300-700 mm to match transformer rating and current density. The UHP grade is specified where high current density, ash ≤ 0.3%, and flexural strength ≥ 10 MPa are needed to limit breakage and tip spalling under arc instability; HP suits lighter duty. Each shipment ships with COA and MTC. Multi-regional sourcing supports CIF Marmara delivery, 20 MT FCL. Send diameter, grade, and nipple connection for a firm RFQ.

Technical Specifications

Diameter300-700mmGradeUHP / HPBulk Density≥ 1.68 g/cm³Resistivity≤ 5.8 µΩ·m

Applications

EAF steelmakingLadle furnace (LF)Submerged-arc furnace
DetailsAvailable on Request
Carbon Electrode Paste (Söderberg)Out of StockNEW

Carbon Electrode Paste (Söderberg)

Electrode PasteCarbon Products

Söderberg electrode paste is a self-baking carbon mix of calcined anthracite, electrically calcined coal, and coke aggregate bound with coal-tar pitch. Charged into the casing of a continuous electrode, it softens at 70-110°C, flows to fill the column, then bakes in situ from furnace heat into a solid conductor. Controlled volatile matter (V.M 12-15.5%) escapes cleanly during that bake; a softening point held in this band prevents green-paste segregation and electrode breaks during slipping. Low resistivity (≤ 75 µΩ·m) and compressive strength ≥ 18 MPa let the column carry high current density and resist soft-tip and hard-break failures. The paste feeds submerged-arc furnaces for ferroalloy smelting (FeSi, FeMn, SiMn, FeCr) and calcium carbide production, where the self-baking electrode eliminates the pre-baked, machined graphite electrode. Fixed carbon ≥ 80% with ash ≤ 8% limits ash carry-over into the bath. Paste is graded standard or sealing/closed-top by V.M and softening point to match electrode diameter and slipping rate. Supplied with COA and MTC, multi-regional sourcing, CIF Marmara, 20 MT FCL. Send diameter and current rating for a graded RFQ.

Technical Specifications

F.C≥ 80%Ash≤ 8%V.M12-15.5%Resistivity≤ 75 µΩ·m

Applications

Submerged-arc furnacesFerroalloy smeltingCalcium carbide production
DetailsAvailable on Request
Carbon Raiser (Calcined Anthracite)Out of StockNEW

Carbon Raiser (Calcined Anthracite)

CACCarbon Products

Calcined anthracite carbon raiser (CAC) is a thermally treated anthracite recarburizer that raises the carbon level of molten iron and steel. Calcination drives off volatiles and orders the carbon structure, so fixed carbon dissolves into the melt and lifts final C toward target chemistry without the cost of graphitized grades. With F.C 90-95% and a graphite-poor structure, recovery sits below synthetic graphite, which is precisely why it serves as an economical bulk carbon tier where premium pickup is not required. Typical use: grey and ductile iron carburization, casting recarburization, and EAF charge carbon for construction steel, dosed roughly 0.5-2.0 wt% depending on charge carbon deficit and target grade. The spec set supports controlled, low-residual additions: S ≤ 0.3% protects nodularity, Ash ≤ 4%, V.M ≤ 1.0%, Moisture ≤ 1.0%, N ≤ 300 ppm to limit pinholing, sized 1-5 mm for steady dissolution. Supplied with COA and MTC, multi-regional sourcing, CIF Marmara, 20 MT FCL. Send target chemistry and tonnage for an RFQ.

Technical Specifications

F.C90-95%S≤ 0.3%Ash≤ 4%V.M≤ 1.0%

Applications

Grey & ductile iron carburizationEAF charge carbonCasting recarburization
DetailsAvailable on Request